Bennewart Flexing Test
Observation 3.5mm cut growth was observed after 30,000 cycles
Requirements 4mm (max) cut growth after 30,000 cycles
Interlayer Bond Strength
Value 4.22 N/mm
Requirements 3.00 N/mm (minimum)
Abrasion Resistance
Volume Loss in mm 3 56.09 mm3
Requirements 250 mm3 (maximum)
Ross Flex after Hydolysis
Observation 2 mm cut growht was observed in sample till 150,000 cycles
Requirements 4 mm(max) cut growth after 150,000 cycles
Tear Strength
Value 10kN/m
Requirements 5kN/m